Ex-situ observation on the dissolution behaviour of Ni–16Cr–15Mo and Ni–30Co–16Cr–15Mo alloys in hydrofluoric acid
点击次数:
影响因子:7.205
DOI码:10.1016/j.corsci.2014.10.003
所属单位:Cent S Univ
发表刊物:Corros Sci
合写作者:Chen Zhang, Akihiko Chiba
第一作者:Yuhang Hou
论文类型:基础研究
通讯作者:Yunping Li
论文编号:72
一级学科:材料学
文献类型:J
卷号:90
页面范围:133-139
是否译文:否
发表时间:2015-02-01
上一条:Phase and grain size inhomogeneity and their influences on creep behavior of Co-Cr-Mo alloy additive manufactured by electron-beam melting (EBM)