Selective separation and recovery of iron and tin from high calcium type tin-, iron-bearing tailings using magnetizing roasting followed by magnetic separation
发布时间:2016-07-05
点击次数:
所属单位:Central South University
发表刊物:Separation Science and Technology
关键字:High calcium type tin- andiron-bearing tailings;cassiterite; magnetizingroasting; magneticseparation
摘要:In this study, a process of magnetizing roasting followed by magnetic separation, which is used to separate or recover tin and iron from the high calcium type tin- and iron-bearing tailings (containing 35.53 wt.% Fe and 0.56 wt.% Sn), was investigated . A magnetic concentrate containing 66.3 wt.% Fe and 0.07 wt.% Sn with an iron recovery rate of 92.9 wt.% was obtained under optimal conditions:anthracite ratio of 2.5:100, roasting temperature of 850°C, roasting time of 30 min, grinding time of 10 min, and magnetic field intensity of 0.1 T.
合写作者:Tao Jiang, Guanghui Li, Bingbing Liu, Jun Chen, Yuanbo Zhang*, Zijian Su
论文类型:基础研究